Final Magnetic Moment2.376 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom1.033 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.052 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeMg3 + Ce |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 0 0> | 144.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 295.3 |
C (mp-48) | <1 0 1> | <1 0 1> | 179.7 |
C (mp-48) | <1 1 1> | <1 0 1> | 314.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 26.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 72.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 224.7 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 124.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 107.4 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 314.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 322.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 252.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 180.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 89.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 214.7 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 224.7 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 124.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 288.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 187.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 252.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 144.1 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 124.8 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 179.7 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 224.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 161.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 180.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 53.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 271.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 322.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 187.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 224.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 80.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 161.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 26.8 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 314.5 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 252.2 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 187.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 180.2 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 1> | 134.8 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 0> | 288.3 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 252.2 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 0> | 252.2 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 124.8 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 179.7 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 224.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 144.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 241.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 134.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 80.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 187.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
InAgS2 (mp-676113) | 0.0750 | 0.208 | 3 |
Li2CrO3 (mp-769794) | 0.7013 | 0.007 | 3 |
HfMgN2 (mp-1029834) | 0.2713 | 0.000 | 3 |
MgTiN2 (mp-1029702) | 0.4071 | 0.023 | 3 |
MgZrN2 (mp-1029536) | 0.2468 | 0.026 | 3 |
Li2AlFeO4 (mp-772430) | 0.6411 | 0.150 | 4 |
Li4Ti3VO8 (mp-763707) | 0.5367 | 0.102 | 4 |
LiAlNiO3 (mp-770087) | 0.7139 | 0.081 | 4 |
LiFe5O5F (mp-766142) | 0.3870 | 0.067 | 4 |
Li2MnOF2 (mp-767979) | 0.4038 | 0.083 | 4 |
YbSe (mp-10648) | 0.0158 | 0.143 | 2 |
TiP (mp-696572) | 0.0291 | 0.281 | 2 |
ScC (mp-999205) | 0.0137 | 0.579 | 2 |
SrMg (mp-1094712) | 0.0162 | 0.562 | 2 |
Ba (mp-1008283) | 0.2009 | 0.728 | 1 |
Ba (mp-1061724) | 0.1871 | 0.728 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Mg_pv |
Final Energy/Atom-2.7336 eV |
Corrected Energy-10.9344 eV
-10.9344 eV = -10.9344 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)