Final Magnetic Moment0.955 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.972 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.048 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMg149 + Li2HfO3 + Hf + MgO |
Band Gap0.485 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmm2 [25] |
HallP 2 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 146.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 292.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 219.1 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 103.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.0 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 103.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 292.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 146.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 206.8 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 73.0 |
InP (mp-20351) | <1 1 0> | <0 1 1> | 103.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 292.2 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 126.7 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 103.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 219.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 146.1 |
Al (mp-134) | <1 1 0> | <0 1 1> | 206.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 219.1 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 292.2 |
TeO2 (mp-2125) | <0 1 0> | <0 1 1> | 206.8 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 206.8 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 292.2 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 73.0 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 1> | 103.4 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 126.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 73.0 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 103.4 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 126.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 219.1 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 219.1 |
Al2O3 (mp-1143) | <1 1 0> | <0 0 1> | 219.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 73.0 |
PbS (mp-21276) | <1 1 0> | <0 1 1> | 103.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 292.6 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 292.2 |
Si (mp-149) | <1 0 0> | <0 0 1> | 146.1 |
Au (mp-81) | <1 0 0> | <0 0 1> | 292.2 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 219.1 |
C (mp-66) | <1 1 1> | <0 0 1> | 219.1 |
Cu (mp-30) | <1 1 0> | <0 1 1> | 206.8 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 292.2 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 219.1 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 146.1 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 292.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 292.2 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 73.0 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 292.2 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 292.2 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 219.1 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 292.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn(Ni9O10)2 (mp-763814) | 0.3276 | 0.028 | 3 |
Li9Co9O17 (mp-735506) | 0.4403 | 0.122 | 3 |
Li14Co13O28 (mp-777836) | 0.3970 | 0.137 | 3 |
Li11(NiO2)12 (mp-38676) | 0.4394 | 0.009 | 3 |
Li11(NiO2)12 (mp-698713) | 0.3638 | 0.009 | 3 |
NaHfMg30O31 (mp-1098489) | 0.0710 | 0.104 | 4 |
NaHfMg30O31 (mp-1098490) | 0.0959 | 0.117 | 4 |
LiHfMg30O31 (mp-1098433) | 0.0820 | 0.107 | 4 |
NaHfMg30O31 (mp-1039713) | 0.0729 | 0.104 | 4 |
LiHfMg30O31 (mp-1039957) | 0.0838 | 0.107 | 4 |
Fe35O36 (mp-694910) | 0.3074 | 0.784 | 2 |
Sc20O19 (mp-684697) | 0.2523 | 0.060 | 2 |
Fe38O39 (mp-705753) | 0.2576 | 0.071 | 2 |
Ni15Cl16 (mp-1094137) | 0.3744 | 0.277 | 2 |
Sc16O15 (mp-759946) | 0.3356 | 0.054 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Hf_pv Mg_pv O |
Final Energy/Atom-6.0096 eV |
Corrected Energy-399.9036 eV
Uncorrected energy = -378.6066 eV
Composition-based energy adjustment (-0.687 eV/atom x 31.0 atoms) = -21.2970 eV
Corrected energy = -399.9036 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)