Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.152 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.030 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 139.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 257.8 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 231.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 225.6 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 192.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 199.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 231.7 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 233.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 166.4 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 99.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 199.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 323.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 278.0 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 66.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 233.1 |
Al (mp-134) | <1 0 0> | <0 1 1> | 231.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 233.1 |
Al (mp-134) | <1 1 1> | <0 1 0> | 199.8 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 231.7 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 139.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 225.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 199.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 199.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 66.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 194.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 320.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 192.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 266.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 231.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 129.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 290.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 96.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 1> | 278.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 221.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 193.4 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 278.0 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 290.1 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 299.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 323.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 225.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 290.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 193.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 258.7 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 66.6 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 231.7 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 332.7 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 332.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 323.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 257.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YSiAu (mp-9025) | 0.5740 | 0.000 | 3 |
SmAsPd (mp-8951) | 0.5726 | 0.000 | 3 |
GdCuGe (mp-13212) | 0.5700 | 0.000 | 3 |
CeGeAu (mp-4219) | 0.5798 | 0.040 | 3 |
PrSiPd (mp-29565) | 0.5711 | 0.000 | 3 |
LaSi2 (mp-2062) | 0.7076 | 0.000 | 2 |
TbZn2 (mp-2338) | 0.6996 | 0.000 | 2 |
BaGe2 (mp-2611) | 0.6429 | 0.025 | 2 |
SrSi2 (mp-1727) | 0.6671 | 0.000 | 2 |
PrGe2 (mp-1077183) | 0.7115 | 0.044 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce As Rh_pv |
Final Energy/Atom-7.1291 eV |
Corrected Energy-85.5492 eV
Uncorrected energy = -85.5492 eV
Corrected energy = -85.5492 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)