Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.451 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBOs + ScB2Os |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 140.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 204.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 263.0 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 228.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 280.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 319.6 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 175.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 140.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 315.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 273.9 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 137.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 263.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 204.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 263.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 315.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 87.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 315.7 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 350.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 105.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 315.7 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 137.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 280.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 263.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 140.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 58.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 321.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 315.7 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 273.9 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 137.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 280.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 315.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 233.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 204.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 321.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 204.5 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 263.0 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 116.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 204.5 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 91.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 273.9 |
Te2W (mp-22693) | <1 1 0> | <0 1 1> | 228.3 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 146.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 175.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 273.9 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 273.9 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 273.9 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 228.3 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 175.3 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 91.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 137.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CeCu4Sn (mp-655580) | 0.6879 | 0.291 | 3 |
Tl5Se2Cl (mp-28920) | 0.6501 | 0.000 | 3 |
Eu(Ni5P3)2 (mp-21672) | 0.7007 | 0.000 | 3 |
MgB4Os3 (mp-10503) | 0.1642 | 0.000 | 3 |
Ba(Ni5P3)2 (mp-14765) | 0.6838 | 0.006 | 3 |
Nb3Te4 (mp-7564) | 0.6597 | 0.000 | 2 |
Nb3Se4 (mp-561) | 0.6840 | 0.000 | 2 |
Sn3Ru2 (mp-680677) | 0.6467 | 0.002 | 2 |
Ge3Ru2 (mp-706531) | 0.6446 | 0.003 | 2 |
Ge3Os2 (mp-510032) | 0.6476 | 0.012 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sc_sv B Os_pv |
Final Energy/Atom-8.7922 eV |
Corrected Energy-140.6755 eV
-140.6755 eV = -140.6755 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)