Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.386 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 109.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 127.0 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 317.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 63.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 89.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 317.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 253.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 179.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 317.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 317.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 317.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 127.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 89.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 63.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 63.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 89.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 317.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 317.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 317.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 253.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 253.9 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 179.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 317.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 269.3 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 317.4 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 317.4 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 89.8 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 317.4 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 179.5 |
BN (mp-984) | <0 0 1> | <1 0 0> | 190.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 190.4 |
BN (mp-984) | <1 0 1> | <1 1 0> | 179.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 317.4 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 269.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 190.4 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 190.4 |
NdGaO3 (mp-3196) | <1 0 0> | <1 1 0> | 89.8 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 190.4 |
Si (mp-149) | <1 1 0> | <1 0 0> | 127.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 317.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 317.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 190.4 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 179.5 |
Au (mp-81) | <1 0 0> | <1 0 0> | 317.4 |
Au (mp-81) | <1 1 0> | <1 1 0> | 269.3 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 317.4 |
WS2 (mp-224) | <1 1 1> | <1 0 0> | 317.4 |
C (mp-48) | <1 1 0> | <1 1 0> | 269.3 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 190.4 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 269.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
86 | 61 | 61 | 0 | 0 | 0 |
61 | 86 | 61 | 0 | 0 | 0 |
61 | 61 | 86 | 0 | 0 | 0 |
0 | 0 | 0 | 37 | 0 | 0 |
0 | 0 | 0 | 0 | 37 | 0 |
0 | 0 | 0 | 0 | 0 | 37 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
27.9 | -11.5 | -11.5 | 0 | 0 | 0 |
-11.5 | 27.9 | -11.5 | 0 | 0 | 0 |
-11.5 | -11.5 | 27.9 | 0 | 0 | 0 |
0 | 0 | 0 | 27.1 | 0 | 0 |
0 | 0 | 0 | 0 | 27.1 | 0 |
0 | 0 | 0 | 0 | 0 | 27.1 |
Shear Modulus GV27 GPa |
Bulk Modulus KV69 GPa |
Shear Modulus GR21 GPa |
Bulk Modulus KR69 GPa |
Shear Modulus GVRH24 GPa |
Bulk Modulus KVRH69 GPa |
Elastic Anisotropy1.50 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbNi4Au (mp-1024977) | 0.0000 | 0.040 | 3 |
TmInCu4 (mp-1024957) | 0.0028 | 0.000 | 3 |
GdNi4Au (mp-1077131) | 0.0027 | 0.855 | 3 |
YbCu4Au (mp-1077165) | 0.0028 | 0.000 | 3 |
GdInCu4 (mp-1077293) | 0.0009 | 0.000 | 3 |
DyMn2 (mp-2483) | 0.0000 | 0.144 | 2 |
PrNi2 (mp-2016) | 0.0000 | 0.012 | 2 |
NdPt2 (mp-2720) | 0.0000 | 0.000 | 2 |
TiCr2 (mp-1425) | 0.0000 | 0.000 | 2 |
LuNi2 (mp-2130) | 0.0000 | 0.000 | 2 |
Co (mp-1072089) | 0.0000 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Au |
Final Energy/Atom-3.0063 eV |
Corrected Energy-18.0381 eV
-18.0381 eV = -18.0381 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)