material

Y(AlGe)2

ID:

mp-10521

DOI:

10.17188/1187177


Tags: Yttrium aluminium germanide (1/2/2)

Material Details

Final Magnetic Moment
0.019 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.379 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.021 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.53 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
YAlGe + Ge + Al
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 39053 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Si (mp-149) <1 1 1> <0 0 1> 0.000 207.3
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.000 207.3
Ni (mp-23) <1 1 1> <0 0 1> 0.004 63.8
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.011 303.0
CdTe (mp-406) <1 1 1> <0 0 1> 0.013 303.0
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.016 223.2
InSb (mp-20012) <1 1 1> <0 0 1> 0.020 303.0
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.022 143.5
SiC (mp-11714) <1 0 0> <1 0 0> 0.025 312.5
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.028 340.9
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.029 207.3
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.030 207.3
C (mp-48) <0 0 1> <0 0 1> 0.034 15.9
MgO (mp-1265) <1 0 0> <0 0 1> 0.036 127.6
TiO2 (mp-2657) <1 1 0> <1 1 0> 0.038 98.4
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.038 111.6
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.039 198.9
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.042 198.9
SiO2 (mp-6930) <1 0 1> <0 0 1> 0.049 318.9
AlN (mp-661) <1 1 0> <0 0 1> 0.053 191.3
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.057 207.3
ZrO2 (mp-2858) <1 1 1> <0 0 1> 0.062 255.1
Te2Mo (mp-602) <1 1 1> <1 0 0> 0.068 284.1
Mg (mp-153) <1 0 0> <0 0 1> 0.073 334.8
GaN (mp-804) <1 1 0> <1 0 1> 0.075 293.2
SiC (mp-11714) <1 1 0> <0 0 1> 0.076 271.1
AlN (mp-661) <1 0 1> <1 1 0> 0.077 196.8
PbS (mp-21276) <1 1 0> <0 0 1> 0.077 255.1
InSb (mp-20012) <1 1 0> <1 1 0> 0.082 246.1
Ag (mp-124) <1 1 1> <0 0 1> 0.082 207.3
PbS (mp-21276) <1 0 0> <0 0 1> 0.083 255.1
CdWO4 (mp-19387) <1 0 0> <1 0 0> 0.083 312.5
Al (mp-134) <1 1 1> <0 0 1> 0.084 111.6
AlN (mp-661) <0 0 1> <0 0 1> 0.085 111.6
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.087 175.4
MgO (mp-1265) <1 1 0> <0 0 1> 0.088 127.6
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.089 142.1
SiC (mp-8062) <1 1 1> <0 0 1> 0.090 303.0
GaP (mp-2490) <1 1 1> <0 0 1> 0.094 207.3
LaF3 (mp-905) <1 0 0> <0 0 1> 0.095 159.4
TePb (mp-19717) <1 1 1> <0 0 1> 0.103 303.0
YVO4 (mp-19133) <1 0 0> <1 0 0> 0.115 227.3
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.127 159.4
BN (mp-984) <1 1 0> <1 0 0> 0.127 198.9
Cu (mp-30) <1 1 1> <0 0 1> 0.143 207.3
CdWO4 (mp-19387) <1 1 1> <1 0 1> 0.145 260.6
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.147 312.5
GaN (mp-804) <0 0 1> <0 0 1> 0.148 63.8
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.148 284.1
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.152 207.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
107 53 50 -16 0 0
53 107 50 16 0 0
50 50 123 0 0 0
-16 16 0 52 0 0
0 0 0 0 52 -16
0 0 0 0 -16 27
Compliance Tensor Sij (10-12Pa-1)
15.4 -6.9 -3.5 6.9 0 0
-6.9 15.4 -3.5 -6.9 0 0
-3.5 -3.5 11 0 0 0
6.9 -6.9 0 23.5 0 0
0 0 0 0 23.5 13.8
0 0 0 0 13.8 44.6
Shear Modulus GV
39 GPa
Bulk Modulus KV
72 GPa
Shear Modulus GR
30 GPa
Bulk Modulus KR
71 GPa
Shear Modulus GVRH
34 GPa
Bulk Modulus KVRH
71 GPa
Elastic Anisotropy
1.39
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Tb(AlGe)2 (mp-7157) 0.0155 0.000 3
Dy(AlSi)2 (mp-7121) 0.0491 0.009 3
Y(AlSi)2 (mp-10435) 0.0697 0.008 3
Tb(AlSi)2 (mp-10436) 0.0596 0.005 3
Er(AlGe)2 (mp-13069) 0.0488 0.000 3
Li6Mn(FeO3)2 (mp-764386) 0.6958 0.040 4
LiFeCuS2 (mp-755288) 0.7171 0.262 4
Pm2O3 (mp-547622) 0.3086 0.035 2
Pr2O3 (mp-2063) 0.3002 0.026 2
La2O3 (mp-1968) 0.3088 0.024 2
Nd2O3 (mp-2763) 0.3069 0.030 2
Ac2O3 (mp-11107) 0.2952 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Al Ge_d
Final Energy/Atom
-5.0176 eV
Corrected Energy
-25.0879 eV
-25.0879 eV = -25.0879 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 608030
  • 39053
Submitted by
User remarks:
  • Yttrium aluminium germanide (1/2/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)