Final Magnetic Moment0.012 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.052 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.052 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSc |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr22Ni50Mo3 (mp-767825) | 0.1722 | 0.006 | 3 |
TiAgHg2 (mp-30341) | 0.1698 | 0.141 | 3 |
ZnCu2Ni (mp-30593) | 0.1698 | 0.005 | 3 |
CaYMg6 (mp-1023366) | 0.1677 | 0.037 | 3 |
FeNiPt2 (mp-13463) | 0.1520 | 0.000 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.1558 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.2501 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3114 | 0.193 | 4 |
Ni2Mo (mp-784630) | 0.0871 | 0.006 | 2 |
LuAg4 (mp-568953) | 0.1036 | 0.000 | 2 |
CuPt (mp-644311) | 0.0955 | 0.000 | 2 |
NbPd2 (mp-1018151) | 0.0928 | 0.000 | 2 |
CdPt3 (mp-1067236) | 0.1045 | 0.000 | 2 |
Xe (mp-972256) | 0.1481 | 0.000 | 1 |
Ce (mp-567332) | 0.1295 | 0.000 | 1 |
Pr (mp-567630) | 0.0751 | 0.008 | 1 |
Si (mp-1094057) | 0.1633 | 0.518 | 1 |
Ca (mp-45) | 0.1337 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sc_sv |
Final Energy/Atom-6.2800 eV |
Corrected Energy-6.2800 eV
-6.2800 eV = -6.2800 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)