Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.029 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.029 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPr |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.2756 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.1388 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3867 | 0.193 | 4 |
SmY3 (mp-979292) | 0.0176 | 0.012 | 2 |
TmZr (mp-979011) | 0.0169 | 0.061 | 2 |
Ni3S (mp-976881) | 0.0196 | 0.371 | 2 |
YZr (mp-971933) | 0.0211 | 0.113 | 2 |
ReOs3 (mp-867141) | 0.0212 | 0.000 | 2 |
Be (mp-87) | 0.0254 | 0.000 | 1 |
Ru (mp-33) | 0.0225 | 0.000 | 1 |
Os (mp-49) | 0.0239 | 0.000 | 1 |
Fe (mp-136) | 0.0302 | 0.098 | 1 |
Sc (mp-1057622) | 0.0366 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 |
Final Energy/Atom-4.7520 eV |
Corrected Energy-9.5039 eV
-9.5039 eV = -9.5039 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)