Final Magnetic Moment0.114 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.310 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6/mmm [191] |
Hall-P 6 2 |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 302.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 302.6 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 137.5 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 110.0 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 208.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 137.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 120.4 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 146.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 220.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 150.3 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 293.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 137.6 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 275.2 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 330.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 326.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 279.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 64.4 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 183.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 154.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 357.6 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 146.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 137.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 107.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 146.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 208.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 326.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 279.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 189.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 357.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 275.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 189.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 171.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 192.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 220.1 |
InAs (mp-20305) | <1 0 0> | <1 1 1> | 36.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 208.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.4 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 293.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 137.6 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 275.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 146.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 68.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 85.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 64.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 206.4 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 257.0 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 344.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 326.8 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 146.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
117 | 37 | 36 | 0 | 0 | 0 |
37 | 117 | 36 | 0 | 0 | 0 |
36 | 36 | 70 | 0 | 0 | 0 |
0 | 0 | 0 | 25 | 0 | 0 |
0 | 0 | 0 | 0 | 25 | 0 |
0 | 0 | 0 | 0 | 0 | 40 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
10.5 | -2 | -4.3 | 0 | 0 | 0 |
-2 | 10.5 | -4.3 | 0 | 0 | 0 |
-4.3 | -4.3 | 18.7 | 0 | 0 | 0 |
0 | 0 | 0 | 40.8 | 0 | 0 |
0 | 0 | 0 | 0 | 40.8 | 0 |
0 | 0 | 0 | 0 | 0 | 25 |
Shear Modulus GV31 GPa |
Bulk Modulus KV58 GPa |
Shear Modulus GR29 GPa |
Bulk Modulus KR54 GPa |
Shear Modulus GVRH30 GPa |
Bulk Modulus KVRH56 GPa |
Elastic Anisotropy0.42 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiAlPt (mp-1025063) | 0.2826 | 0.102 | 3 |
MnNiGe (mp-21090) | 0.3641 | 0.030 | 3 |
YbHgPb (mp-571493) | 0.3613 | 0.082 | 3 |
MnNiGe (mp-583202) | 0.3610 | 0.323 | 3 |
CeTlCd (mp-1018668) | 0.1254 | 0.052 | 3 |
TbCd2 (mp-1063176) | 0.0592 | 0.000 | 2 |
NdCd2 (mp-1097979) | 0.0235 | 0.000 | 2 |
TiS2 (mp-1008676) | 0.0464 | 1.284 | 2 |
PrCd2 (mp-2324) | 0.0374 | 0.000 | 2 |
ThAg2 (mp-309) | 0.0396 | 0.000 | 2 |
Ti (mp-72) | 0.6951 | 0.000 | 1 |
Hf (mp-1009460) | 0.7055 | 0.045 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 Cd |
Final Energy/Atom-2.4606 eV |
Corrected Energy-7.3817 eV
-7.3817 eV = -7.3817 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)