Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.712 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTiS2 |
Band Gap0.050 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnCoO4 (mp-766792) | 0.4792 | 0.056 | 3 |
Co3NiO8 (mp-765936) | 0.4711 | 0.038 | 3 |
Co3NiO8 (mp-765866) | 0.4831 | 0.081 | 3 |
Li2UBr6 (mp-531472) | 0.4878 | 0.000 | 3 |
Li(TiS2)3 (mp-19755) | 0.4800 | 0.015 | 3 |
LiV2OF5 (mp-767433) | 0.7175 | 0.055 | 4 |
LiV3(OF3)2 (mp-766156) | 0.7106 | 0.082 | 4 |
NaLa6OsI12 (mp-569905) | 0.6915 | 0.000 | 4 |
LiMnFeF6 (mp-566418) | 0.7074 | 0.000 | 4 |
LiTiMnF6 (mp-556715) | 0.7188 | 0.513 | 4 |
TiBr2 (mp-27785) | 0.3029 | 0.057 | 2 |
TiS2 (mvc-11238) | 0.2600 | 0.010 | 2 |
CrS2 (mp-28910) | 0.0091 | 0.008 | 2 |
CrS2 (mp-849082) | 0.0134 | 0.008 | 2 |
CrSe2 (mp-1061769) | 0.1080 | 0.015 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv S |
Final Energy/Atom-6.6587 eV |
Corrected Energy-21.3031 eV
-21.3031 eV = -19.9762 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)