Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.004 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.221 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTa5S8 + Ta3S2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6m2 [187] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 142.1 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 129.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 185.9 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 295.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 174.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 218.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 233.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 142.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 201.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 149.2 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 132.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 76.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 149.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 158.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 196.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 139.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 143.7 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 287.4 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 174.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 94.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 177.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 9.3 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 86.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 158.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 289.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 93.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 185.9 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 261.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 94.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 111.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 28.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 273.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 262.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 132.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 189.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 284.1 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 132.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 177.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 94.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 111.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 196.8 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 287.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 240.6 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 258.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaNbSe2 (mp-7939) | 0.6654 | 0.000 | 3 |
NaNbS2 (mp-7937) | 0.6825 | 0.000 | 3 |
LiNbSe2 (mp-1025496) | 0.6248 | 0.000 | 3 |
Ca3SiBr2 (mp-567974) | 0.6284 | 0.252 | 3 |
FeWN2 (mp-29076) | 0.6484 | 0.095 | 3 |
TiO (mp-755264) | 0.0772 | 0.098 | 2 |
WN (mp-991) | 0.0232 | 0.288 | 2 |
TcB (mp-1002188) | 0.0382 | 0.103 | 2 |
ZrTe (mp-1539) | 0.0575 | 0.000 | 2 |
NbS (mp-2243) | 0.0767 | 0.083 | 2 |
Xe (mp-979286) | 0.7274 | 0.006 | 1 |
N2 (mp-1061298) | 0.2646 | 0.000 | 1 |
Li (mp-604313) | 0.6436 | 0.262 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv S |
Final Energy/Atom-8.6690 eV |
Corrected Energy-18.0014 eV
-18.0014 eV = -17.3379 eV (uncorrected energy) - 0.6635 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)