Final Magnetic Moment6.876 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.077 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.038 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGa3Fe + GaFe3 + Mn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mmm [123] |
Hall-P 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GaCo2Ni (mp-20551) | 0.0278 | 0.080 | 3 |
ZnCu2Ni (mp-30593) | 0.2440 | 0.005 | 3 |
Cr11Ni40Mo9 (mp-771746) | 0.3006 | 0.031 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2920 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3612 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.4045 | 0.193 | 4 |
RbBa3 (mp-975509) | 0.0121 | 0.124 | 2 |
LiHo3 (mp-973741) | 0.0031 | 0.198 | 2 |
Nb3Ni (mp-999394) | 0.0123 | 0.213 | 2 |
Li3Mg (mp-1094159) | 0.0151 | 0.002 | 2 |
Mg3Sn (mp-1094514) | 0.0000 | 0.049 | 2 |
Na (mp-974920) | 0.0301 | 0.013 | 1 |
Rb (mp-975519) | 0.0435 | 0.017 | 1 |
Tl (mp-151) | 0.0419 | 0.011 | 1 |
Sn (mp-623511) | 0.0880 | 0.061 | 1 |
In (mp-1055994) | 0.0659 | 0.030 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mn_pv Ga_d Fe_pv |
Final Energy/Atom-7.3594 eV |
Corrected Energy-29.4375 eV
-29.4375 eV = -29.4375 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)