Final Magnetic Moment2.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.100 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.212 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVCoAs + Fe |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
PmDyRu2 (mp-983429) | 0.0000 | 0.000 | 3 |
BeBiOs2 (mp-631507) | 0.0000 | 1.050 | 3 |
SrLaZr2 (mp-631340) | 0.0000 | 0.605 | 3 |
GaTc2W (mp-865746) | 0.0000 | 0.000 | 3 |
MnFe2Si (mp-1001159) | 0.0000 | 0.000 | 3 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoSi (mp-998971) | 0.0000 | 0.029 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VGaFeCo (mp-1066581) | 0.0000 | 0.029 | 4 |
AlVFeCo (mp-1008530) | 0.0000 | 0.029 | 4 |
NaYb3 (mp-980189) | 0.0000 | 0.083 | 2 |
NaCd3 (mp-865077) | 0.0000 | 0.000 | 2 |
Nb3Ni (mp-999396) | 0.0000 | 0.134 | 2 |
Ti3Ga (mp-998988) | 0.0000 | 0.129 | 2 |
Rb3Al (mp-975052) | 0.0000 | 0.365 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: V_pv Fe_pv Co As |
Final Energy/Atom-7.4300 eV |
Corrected Energy-29.7200 eV
-29.7200 eV = -29.7200 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)