Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.821 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.625 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.84 | 0.00 | -0.00 |
0.00 | 6.84 | -0.00 |
-0.00 | -0.00 | 7.49 |
Dielectric Tensor εij (total) |
||
---|---|---|
21.75 | 0.00 | -0.00 |
0.00 | 21.75 | -0.00 |
-0.00 | -0.00 | 33.45 |
Polycrystalline dielectric constant
εpoly∞
7.05
|
Polycrystalline dielectric constant
εpoly
25.65
|
Refractive Index n2.66 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
DyTlS2 (mp-31166) | 0.0213 | 0.000 | 3 |
TbTlS2 (mp-999119) | 0.0134 | 0.000 | 3 |
KLuS2 (mp-1007636) | 0.0370 | 0.000 | 3 |
RbSmSe2 (mp-10780) | 0.0384 | 0.000 | 3 |
RbGdSe2 (mp-10781) | 0.0262 | 0.000 | 3 |
Na3Mn2SbO6 (mp-985626) | 0.5891 | 0.361 | 4 |
Na3Ni2SbO6 (mp-971678) | 0.4305 | 0.000 | 4 |
Na2Li(NiO2)3 (mp-773956) | 0.5350 | 0.031 | 4 |
Na3Co2SbO6 (mp-561940) | 0.5464 | 0.015 | 4 |
Na3Co2SbO6 (mp-19087) | 0.4795 | 0.000 | 4 |
Bi8Se7 (mp-680214) | 0.4192 | 0.009 | 2 |
Ag2O (mp-7711) | 0.4274 | 0.120 | 2 |
Bi4Se3 (mp-27607) | 0.4202 | 0.005 | 2 |
TlS (mp-998912) | 0.2719 | 0.062 | 2 |
Bi2Te3 (mp-34202) | 0.4288 | 0.000 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.4886 | 0.139 | 5 |
Na (mp-999501) | 0.6513 | 0.114 | 1 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Tl_d S |
Final Energy/Atom-5.7646 eV |
Corrected Energy-24.0643 eV
Uncorrected energy = -23.0583 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Corrected energy = -24.0643 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)