material

Ba3(AlGe)2

ID:

mp-10669

DOI:

10.17188/1187274


Tags: Aluminum barium germanide (2/3/2)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.468 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.45 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Immm [71]
Hall
-I 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 52612 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InAs (mp-20305) <1 1 0> <0 0 1> 0.001 270.4
ZnTe (mp-2176) <1 1 0> <0 0 1> 0.001 270.4
Te2W (mp-22693) <0 1 0> <0 0 1> 0.005 270.4
SiC (mp-8062) <1 1 0> <0 0 1> 0.006 135.2
BN (mp-984) <1 1 0> <0 0 1> 0.025 67.6
CdSe (mp-2691) <1 1 0> <0 0 1> 0.041 270.4
CdSe (mp-2691) <1 0 0> <0 0 1> 0.041 270.4
GaSb (mp-1156) <1 0 0> <0 0 1> 0.045 270.4
BN (mp-984) <1 1 1> <0 0 1> 0.054 67.6
PbSe (mp-2201) <1 0 0> <0 0 1> 0.054 270.4
GaSb (mp-1156) <1 1 0> <0 0 1> 0.060 270.4
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.062 292.9
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.069 270.4
Cu (mp-30) <1 0 0> <1 0 0> 0.072 104.4
InAs (mp-20305) <1 0 0> <0 0 1> 0.077 270.4
Ag (mp-124) <1 0 0> <0 0 1> 0.084 360.5
PbSe (mp-2201) <1 1 0> <0 0 1> 0.088 270.4
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.090 112.7
Cu (mp-30) <1 1 0> <0 0 1> 0.094 112.7
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.108 292.9
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.114 135.2
CdS (mp-672) <1 1 1> <0 1 0> 0.119 265.1
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.122 270.4
Au (mp-81) <1 1 0> <0 0 1> 0.124 225.3
Au (mp-81) <1 0 0> <0 0 1> 0.140 360.5
GaSe (mp-1943) <0 0 1> <0 0 1> 0.140 202.8
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.143 202.8
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.145 360.5
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.151 338.0
LiTaO3 (mp-3666) <1 0 0> <1 0 1> 0.156 213.5
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.159 360.5
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.173 135.2
Ag (mp-124) <1 1 1> <1 0 0> 0.174 208.7
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.189 292.9
MoSe2 (mp-1634) <1 0 0> <0 0 1> 0.196 202.8
CdS (mp-672) <1 0 1> <0 0 1> 0.197 360.5
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.203 112.7
Ag (mp-124) <1 1 0> <0 0 1> 0.208 225.3
Au (mp-81) <1 1 1> <1 0 0> 0.208 208.7
TePb (mp-19717) <1 0 0> <0 0 1> 0.222 338.0
TiO2 (mp-2657) <1 0 0> <0 1 0> 0.234 265.1
SiC (mp-8062) <1 0 0> <0 0 1> 0.237 112.7
ZrO2 (mp-2858) <1 0 -1> <1 0 1> 0.240 106.8
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.241 292.9
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.241 292.9
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.242 157.7
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.242 213.5
SiC (mp-8062) <1 1 1> <0 0 1> 0.254 360.5
CdS (mp-672) <0 0 1> <0 0 1> 0.255 360.5
LiAlO2 (mp-3427) <1 1 1> <0 1 0> 0.259 265.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
60 22 14 0 0 0
22 55 17 0 0 0
14 17 81 0 0 0
0 0 0 13 0 0
0 0 0 0 29 0
0 0 0 0 0 20
Compliance Tensor Sij (10-12Pa-1)
20 -7.4 -1.9 0 0 0
-7.4 22.1 -3.3 0 0 0
-1.9 -3.3 13.3 0 0 0
0 0 0 75.7 0 0
0 0 0 0 34.3 0
0 0 0 0 0 49.8
Shear Modulus GV
22 GPa
Bulk Modulus KV
33 GPa
Shear Modulus GR
20 GPa
Bulk Modulus KR
33 GPa
Shear Modulus GVRH
21 GPa
Bulk Modulus KVRH
33 GPa
Elastic Anisotropy
0.53
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba3(AlSi)2 (mp-9578) 0.1108 0.000 3
Ba3(AlSn)2 (mp-7377) 0.2576 0.006 3
Sr3(AlSn)2 (mp-7376) 0.4662 0.005 3
Sr3(AlSi)2 (mp-7068) 0.2259 0.000 3
Sr3(AlGe)2 (mp-10671) 0.2994 0.000 3
Ti3B4 (mp-1025170) 0.7184 0.000 2
Ta3B4 (mp-10142) 0.7429 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Al Ge_d
Final Energy/Atom
-3.6816 eV
Corrected Energy
-25.7711 eV
-25.7711 eV = -25.7711 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 52612
Submitted by
User remarks:
  • Aluminum barium germanide (2/3/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)