Final Magnetic Moment
0.005 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.512 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.007 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.02 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CaAl2 + CaGe
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Immm [71]
Hall
-I 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 52616 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.010 357.9
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.015 226.0
LiAlO2 (mp-3427) <1 0 1> <0 0 1> 0.027 301.4
WSe2 (mp-1821) <1 0 0> <0 0 1> 0.028 150.7
GaTe (mp-542812) <0 0 1> <0 0 1> 0.029 75.3
SiC (mp-8062) <1 0 0> <1 1 0> 0.037 114.8
ZnTe (mp-2176) <1 0 0> <1 1 0> 0.037 114.8
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.037 150.7
InAs (mp-20305) <1 0 0> <1 1 0> 0.039 114.8
ZrO2 (mp-2858) <1 1 1> <1 0 0> 0.044 255.6
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.061 339.0
ZrO2 (mp-2858) <1 1 -1> <0 0 1> 0.062 226.0
CdSe (mp-2691) <1 0 0> <1 1 0> 0.063 114.8
GaTe (mp-542812) <1 0 -1> <0 0 1> 0.064 75.3
Fe2O3 (mp-24972) <1 0 0> <0 0 1> 0.068 282.5
TeO2 (mp-2125) <1 0 0> <0 0 1> 0.071 282.5
Ag (mp-124) <1 1 0> <0 0 1> 0.074 169.5
GaSb (mp-1156) <1 0 0> <1 1 0> 0.080 114.8
SiC (mp-7631) <1 0 1> <0 0 1> 0.084 94.2
BN (mp-984) <0 0 1> <0 0 1> 0.087 226.0
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.089 263.7
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.095 188.3
PbSe (mp-2201) <1 0 0> <1 1 0> 0.106 114.8
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.113 357.9
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.113 263.7
Si (mp-149) <1 0 0> <0 0 1> 0.115 357.9
InP (mp-20351) <1 0 0> <0 0 1> 0.122 244.8
GaN (mp-804) <1 1 0> <0 1 1> 0.124 317.2
ZrO2 (mp-2858) <1 0 1> <0 0 1> 0.135 301.4
Au (mp-81) <1 1 0> <0 0 1> 0.144 169.5
ZnO (mp-2133) <1 1 1> <0 0 1> 0.148 94.2
LiF (mp-1138) <1 1 0> <0 0 1> 0.152 94.2
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.152 207.2
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.169 320.2
Mg (mp-153) <1 1 1> <0 0 1> 0.170 150.7
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.172 263.7
ZnO (mp-2133) <1 0 0> <0 0 1> 0.176 226.0
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.176 320.2
LaAlO3 (mp-2920) <1 0 0> <0 0 1> 0.178 282.5
C (mp-48) <1 1 1> <0 0 1> 0.180 301.4
AlN (mp-661) <1 1 0> <0 0 1> 0.181 357.9
LaAlO3 (mp-2920) <1 1 0> <0 0 1> 0.186 244.8
C (mp-48) <0 0 1> <0 0 1> 0.187 169.5
NaCl (mp-22862) <1 1 0> <0 0 1> 0.190 226.0
Mg (mp-153) <1 0 0> <0 0 1> 0.193 131.8
SiC (mp-11714) <1 0 0> <0 0 1> 0.193 339.0
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.203 85.2
C (mp-66) <1 0 0> <0 0 1> 0.209 282.5
GaTe (mp-542812) <1 0 0> <0 0 1> 0.216 131.8
TePb (mp-19717) <1 1 0> <0 0 1> 0.224 244.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
73 23 19 0 0 0
23 106 24 0 0 0
19 24 120 0 0 0
0 0 0 34 0 0
0 0 0 0 34 0
0 0 0 0 0 25
Compliance Tensor Sij (10-12Pa-1)
15 -2.8 -1.8 0 0 0
-2.8 10.4 -1.6 0 0 0
-1.8 -1.6 8.9 0 0 0
0 0 0 29.3 0 0
0 0 0 0 29.5 0
0 0 0 0 0 39.5
Shear Modulus GV
34 GPa
Bulk Modulus KV
48 GPa
Shear Modulus GR
33 GPa
Bulk Modulus KR
46 GPa
Shear Modulus GVRH
34 GPa
Bulk Modulus KVRH
47 GPa
Elastic Anisotropy
0.26
Poisson's Ratio
0.21

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca3(AlSi)2 (mp-9577) 0.2013 0.027 3
Ba3(AlSn)2 (mp-7377) 0.4645 0.007 3
Sr3(AlSn)2 (mp-7376) 0.2631 0.005 3
Sr3(AlSi)2 (mp-7068) 0.3456 0.000 3
Sr3(AlGe)2 (mp-10671) 0.2693 0.000 3
Mn3B4 (mp-10118) 0.6428 0.043 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Al Ge_d
Final Energy/Atom
-3.7625 eV
Corrected Energy
-26.3376 eV
-26.3376 eV = -26.3376 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 52616
Submitted by
User remarks:
  • Aluminium calcium germanide (2/3/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)