Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.881 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 304.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 112.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 206.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 192.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 137.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 240.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 208.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 303.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 137.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 208.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 64.1 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 189.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 240.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 171.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 304.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 246.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 320.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 341.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 151.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 336.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 240.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 208.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 240.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 171.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 137.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 309.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 192.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 303.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 137.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 274.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 178.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 112.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 16.0 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 151.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 238.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 256.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 272.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 274.8 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 341.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 112.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 288.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 308.1 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 240.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 160.2 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 238.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 309.2 |
YVO4 (mp-19133) | <1 1 1> | <1 1 0> | 238.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 336.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
155 | 85 | 33 | 0 | 0 | 0 |
85 | 155 | 33 | 0 | 0 | 0 |
33 | 33 | 94 | 0 | 0 | 0 |
0 | 0 | 0 | 28 | 0 | 0 |
0 | 0 | 0 | 0 | 28 | 0 |
0 | 0 | 0 | 0 | 0 | 35 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
9.5 | -4.9 | -1.6 | 0 | 0 | 0 |
-4.9 | 9.5 | -1.6 | 0 | 0 | 0 |
-1.6 | -1.6 | 11.8 | 0 | 0 | 0 |
0 | 0 | 0 | 35.8 | 0 | 0 |
0 | 0 | 0 | 0 | 35.8 | 0 |
0 | 0 | 0 | 0 | 0 | 28.7 |
Shear Modulus GV35 GPa |
Bulk Modulus KV79 GPa |
Shear Modulus GR33 GPa |
Bulk Modulus KR69 GPa |
Shear Modulus GVRH34 GPa |
Bulk Modulus KVRH74 GPa |
Elastic Anisotropy0.46 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrAgAs (mp-6954) | 0.0144 | 0.000 | 3 |
TmPPt (mp-7169) | 0.0103 | 0.000 | 3 |
NdPPd (mp-3570) | 0.0103 | 0.000 | 3 |
BaLiSb (mp-10485) | 0.0102 | 0.000 | 3 |
LaPPd (mp-4336) | 0.0040 | 0.000 | 3 |
ThAl2 (mp-669) | 0.0748 | 0.000 | 2 |
TmSi2 (mp-772) | 0.0747 | 0.075 | 2 |
UGa2 (mp-20632) | 0.0795 | 0.246 | 2 |
LuSi2 (mp-1103) | 0.0004 | 0.104 | 2 |
ThNi2 (mp-220) | 0.0931 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv P Au |
Final Energy/Atom-4.4448 eV |
Corrected Energy-26.6688 eV
-26.6688 eV = -26.6688 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)