Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.379 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr(CoP)2 (mp-5671) | 0.0742 | 0.000 | 3 |
Ba(CoAs)2 (mp-20563) | 0.1414 | 0.000 | 3 |
Y2SeO2 (mp-755609) | 0.1396 | 0.054 | 3 |
Dy2SeO2 (mp-769253) | 0.1400 | 0.042 | 3 |
Ce2TeO2 (mp-4873) | 0.1427 | 0.000 | 3 |
KLiZnS2 (mp-774907) | 0.3275 | 0.000 | 4 |
SrBiClO2 (mp-547244) | 0.4553 | 0.000 | 4 |
SrBiBrO2 (mp-552234) | 0.4838 | 0.000 | 4 |
KLiMnS2 (mp-753940) | 0.2645 | 0.000 | 4 |
BiPbClO2 (mp-23084) | 0.2916 | 0.000 | 4 |
Bi3O2 (mp-1022722) | 0.7105 | 0.125 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Co Ge_d |
Final Energy/Atom-5.4535 eV |
Corrected Energy-27.2675 eV
-27.2675 eV = -27.2675 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)