Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.234 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SmCu4Ag (mp-867863) | 0.0027 | 0.000 | 3 |
UAlNi4 (mp-16519) | 0.0028 | 0.047 | 3 |
GdMgNi4 (mp-977381) | 0.0032 | 0.000 | 3 |
YMgCu4 (mp-13172) | 0.0027 | 0.000 | 3 |
CeMgNi4 (mp-13435) | 0.0029 | 0.000 | 3 |
DyCu5 (mp-30578) | 0.0032 | 0.004 | 2 |
HoCu5 (mp-580364) | 0.0052 | 0.007 | 2 |
UCu5 (mp-510148) | 0.0039 | 0.102 | 2 |
TbCu5 (mp-1077262) | 0.0028 | 0.007 | 2 |
ZrNi5 (mp-905383) | 0.0057 | 0.001 | 2 |
Co (mp-1072089) | 0.0375 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Cu_pv Ag |
Final Energy/Atom-4.2109 eV |
Corrected Energy-25.2651 eV
-25.2651 eV = -25.2651 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)