Final Magnetic Moment0.205 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.371 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
UCu4Pd (mp-1071877) | 0.0000 | 0.056 | 3 |
HoCdCu4 (mp-12007) | 0.0000 | 0.000 | 3 |
TmInNi4 (mp-20896) | 0.0006 | 0.000 | 3 |
LuCdNi4 (mp-1077095) | 0.0006 | 0.000 | 3 |
PrInPt4 (mp-1077228) | 0.0006 | 0.000 | 3 |
HfNi5 (mp-569516) | 0.0050 | 0.015 | 2 |
Be5Co (mp-1071690) | 0.0027 | 0.000 | 2 |
ZrCu5 (mp-30603) | 0.0051 | 0.010 | 2 |
Be5Pt (mp-1072399) | 0.0055 | 0.000 | 2 |
UNi5 (mp-2838) | 0.0000 | 0.000 | 2 |
Co (mp-1072089) | 0.0193 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Cd Ni_pv |
Final Energy/Atom-5.1207 eV |
Corrected Energy-30.7240 eV
Uncorrected energy = -30.7240 eV
Corrected energy = -30.7240 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)