Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.091 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.182 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KAg3Se2 (mp-9782) | 0.4741 | 0.000 | 3 |
Pr3RuCl3 (mp-639135) | 0.5559 | 0.000 | 3 |
KSm2Cl5 (mp-568044) | 0.4430 | 0.091 | 3 |
RbAg3Se2 (mp-10477) | 0.4993 | 0.000 | 3 |
Ca3Al2Ge3 (mp-27997) | 0.5614 | 0.000 | 3 |
K2SrCdSb2 (mp-863758) | 0.6790 | 0.000 | 4 |
Gd3NbS3O4 (mp-510057) | 0.6494 | 0.062 | 4 |
Nb2Tl3CuSe12 (mp-570757) | 0.6619 | 0.000 | 4 |
KSr2Cd2Sb3 (mp-866639) | 0.4401 | 0.000 | 4 |
Sm3NbS3O4 (mp-16135) | 0.6617 | 0.004 | 4 |
Mg2Si3 (mp-1073154) | 0.4509 | 0.188 | 2 |
MgSi2 (mp-1073405) | 0.4799 | 0.209 | 2 |
MgSi2 (mp-1073493) | 0.4816 | 0.193 | 2 |
Mg3Si4 (mp-1075198) | 0.4522 | 0.266 | 2 |
Mg3Si4 (mp-1075397) | 0.4771 | 0.335 | 2 |
Rb (mp-640416) | 0.6908 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.8044 eV |
Corrected Energy-76.0884 eV
-76.0884 eV = -76.0884 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)