Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.144 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.221 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V6Cu5Te12 (mp-695001) | 0.6074 | 0.408 | 3 |
Sm3(Ge2Ru)2 (mp-22145) | 0.6021 | 0.000 | 3 |
K3In2As3 (mp-583615) | 0.5999 | 0.000 | 3 |
Na2In2Sb3 (mp-541692) | 0.6073 | 0.010 | 3 |
Na2Ga2As3 (mp-15431) | 0.6197 | 0.000 | 3 |
BaLi4NiO4 (mp-776790) | 0.6190 | 0.105 | 4 |
Ce3NbS3O4 (mp-683997) | 0.6046 | 0.067 | 4 |
Gd3NbS3O4 (mp-510057) | 0.6008 | 0.062 | 4 |
Nb2Tl3CuSe12 (mp-570757) | 0.6014 | 0.000 | 4 |
Sm3NbS3O4 (mp-16135) | 0.6208 | 0.004 | 4 |
MgSi2 (mp-1073371) | 0.4719 | 0.195 | 2 |
MgSi2 (mp-1073428) | 0.4755 | 0.182 | 2 |
Mg3Si4 (mp-1074934) | 0.4581 | 0.198 | 2 |
Mg5Si6 (mp-1075403) | 0.4877 | 0.201 | 2 |
Mg5Si9 (mp-1075724) | 0.4336 | 0.253 | 2 |
Si (mp-676011) | 0.7380 | 0.445 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-4.0043 eV |
Corrected Energy-48.0517 eV
-48.0517 eV = -48.0517 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)