Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.176 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.252 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La2SnSb4 (mp-675535) | 0.6146 | 0.233 | 3 |
BaMg6Fe (mp-1099278) | 0.5793 | 0.391 | 3 |
Mg6ZrC (mp-1022489) | 0.5702 | 0.703 | 3 |
BaYbSn3 (mp-571479) | 0.5399 | 0.000 | 3 |
BaCaSn3 (mp-583645) | 0.5190 | 0.000 | 3 |
Re2Si (mp-669547) | 0.5672 | 0.313 | 2 |
Mg4Si3 (mp-1074349) | 0.5679 | 0.204 | 2 |
Mg4Si3 (mp-1074433) | 0.5769 | 0.176 | 2 |
Mg4Si3 (mp-1074475) | 0.5666 | 0.215 | 2 |
Nd2Sn3 (mp-30290) | 0.4954 | 0.000 | 2 |
Rb (mp-656615) | 0.7413 | 0.023 | 1 |
Rb (mp-640416) | 0.7429 | 0.057 | 1 |
Rb (mp-569688) | 0.7308 | 0.062 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.9745 eV |
Corrected Energy-47.6945 eV
-47.6945 eV = -47.6945 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)