Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.182 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.259 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KAg3Se2 (mp-9782) | 0.5883 | 0.000 | 3 |
Ce7(GePd2)2 (mp-683992) | 0.5729 | 0.190 | 3 |
Tl3AgTe2 (mp-650442) | 0.5502 | 0.000 | 3 |
KSm2Cl5 (mp-568044) | 0.5136 | 0.091 | 3 |
Cs5(KPb6)3 (mp-581775) | 0.4669 | 0.006 | 3 |
K2SrCdSb2 (mp-863758) | 0.7238 | 0.000 | 4 |
Nb2Tl3CuSe12 (mp-570757) | 0.7254 | 0.000 | 4 |
KSr2Cd2Sb3 (mp-866639) | 0.5890 | 0.000 | 4 |
Mg4Si3 (mp-1074518) | 0.4200 | 0.175 | 2 |
Mg4Si3 (mp-1074276) | 0.3970 | 0.137 | 2 |
Mg3Si4 (mp-1075198) | 0.4203 | 0.266 | 2 |
Mg3Si4 (mp-1075240) | 0.4261 | 0.216 | 2 |
Mg3Si4 (mp-1075267) | 0.4235 | 0.215 | 2 |
Rb (mp-640416) | 0.5429 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.9663 eV |
Corrected Energy-94.0545 eV
Uncorrected energy = -95.1905 eV
Composition-based energy adjustment (0.071 eV/atom x 16.0 atoms) = 1.1360 eV
Corrected energy = -94.0545 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)