Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.052 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.168 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CeAgP2 (mp-675111) | 0.5880 | 0.222 | 3 |
Ba2LaCl7 (mp-771963) | 0.6204 | 0.092 | 3 |
Si2Ni5P3 (mp-649521) | 0.6512 | 0.051 | 3 |
K4(TiTe3)3 (mp-30280) | 0.5605 | 0.000 | 3 |
K2SrCl4 (mp-674465) | 0.5384 | 0.027 | 3 |
Rb2CeCu3Te5 (mp-581778) | 0.6248 | 0.093 | 4 |
Mg2Si3 (mp-1073065) | 0.5462 | 0.187 | 2 |
MgSi (mp-1073721) | 0.5046 | 0.147 | 2 |
Mg3Si4 (mp-1075302) | 0.5215 | 0.252 | 2 |
Mg3Si4 (mp-1075371) | 0.5547 | 0.275 | 2 |
Mg3Si2 (mp-1075851) | 0.5592 | 0.197 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.4581 eV |
Corrected Energy-41.0718 eV
Uncorrected energy = -41.4978 eV
Composition-based energy adjustment (0.071 eV/atom x 6.0 atoms) = 0.4260 eV
Corrected energy = -41.0718 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)