Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.098 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.225 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nd3(GeRu)2 (mp-630836) | 0.6101 | 0.000 | 3 |
Na3InSb2 (mp-21547) | 0.5980 | 0.000 | 3 |
Er3CoSi3 (mp-568196) | 0.6020 | 0.000 | 3 |
Na3InBi2 (mp-580161) | 0.6063 | 0.000 | 3 |
Y3Si3Rh (mp-16225) | 0.5908 | 0.000 | 3 |
K2BaCdSb2 (mp-863761) | 0.5447 | 0.000 | 4 |
Dy4In(NiGe2)2 (mp-20748) | 0.5029 | 0.000 | 4 |
Er4In(NiGe2)2 (mp-13508) | 0.5013 | 0.000 | 4 |
Ho4In(NiGe2)2 (mp-13510) | 0.4970 | 0.000 | 4 |
Tm4In(NiGe2)2 (mp-13511) | 0.5138 | 0.000 | 4 |
Mg6Si5 (mp-1073876) | 0.4803 | 0.243 | 2 |
Mg6Si5 (mp-1073992) | 0.4718 | 0.203 | 2 |
Mg5Si6 (mp-1075362) | 0.4697 | 0.200 | 2 |
Mg5Si6 (mp-1075481) | 0.4587 | 0.157 | 2 |
Mg5Si6 (mp-1075582) | 0.3856 | 0.159 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.2379 eV |
Corrected Energy-70.5243 eV
Uncorrected energy = -71.2343 eV
Composition-based energy adjustment (0.071 eV/atom x 10.0 atoms) = 0.7100 eV
Corrected energy = -70.5243 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)