Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.043 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.190 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5Ca7Sn11 (mp-672336) | 0.6502 | 0.038 | 3 |
RbTh3F13 (mp-866684) | 0.5503 | 0.087 | 3 |
BaLaCl5 (mp-772035) | 0.6124 | 0.062 | 3 |
Cs5(KPb6)3 (mp-581775) | 0.6144 | 0.006 | 3 |
Ba6Pr3I19 (mp-570423) | 0.5888 | 0.000 | 3 |
Mg4Si3 (mp-1074263) | 0.4368 | 0.205 | 2 |
Mg2Si (mp-1074644) | 0.4524 | 0.174 | 2 |
Mg2Si (mp-1074700) | 0.4344 | 0.162 | 2 |
Mg4Si3 (mp-1074639) | 0.4403 | 0.174 | 2 |
Mg5Si6 (mp-1075505) | 0.4522 | 0.193 | 2 |
Rb (mp-640416) | 0.6515 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-2.9233 eV |
Corrected Energy-81.8516 eV
-81.8516 eV = -81.8516 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)