Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.021 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.168 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5Ca7Sn11 (mp-672336) | 0.6167 | 0.038 | 3 |
RbTh3F13 (mp-866684) | 0.6651 | 0.087 | 3 |
K5(AsPb)3 (mp-646920) | 0.6725 | 0.000 | 3 |
Ho10In20Ni9 (mp-30729) | 0.6731 | 0.000 | 3 |
Ba6Pr3I19 (mp-570423) | 0.5567 | 0.000 | 3 |
Mg9Si5 (mp-1074026) | 0.4944 | 0.190 | 2 |
Mg4Si3 (mp-1074278) | 0.5236 | 0.199 | 2 |
Mg2Si (mp-1074644) | 0.4737 | 0.174 | 2 |
Mg7Si4 (mp-1074788) | 0.5188 | 0.169 | 2 |
Mg3Si4 (mp-1075282) | 0.5194 | 0.226 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-2.9455 eV |
Corrected Energy-82.4748 eV
-82.4748 eV = -82.4748 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)