Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.000 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.133 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb7Mg3Ge8 (mp-685798) | 0.5434 | 0.256 | 3 |
Bi3O2F5 (mp-759405) | 0.5619 | 0.006 | 3 |
Ca2CdSb2 (mp-569267) | 0.4687 | 0.000 | 3 |
BaSr2I6 (mp-752711) | 0.5646 | 0.057 | 3 |
Yb2CdSb2 (mp-569106) | 0.4768 | 0.000 | 3 |
TiTlCuTe3 (mp-9344) | 0.7077 | 0.000 | 4 |
BaYbCdSb2 (mp-865143) | 0.6716 | 0.000 | 4 |
Sm3NbSe3O4 (mp-555559) | 0.7237 | 0.024 | 4 |
Nb2Tl3CuSe12 (mp-570757) | 0.6737 | 0.000 | 4 |
KSr2Cd2Sb3 (mp-866639) | 0.6590 | 0.000 | 4 |
MgSi2 (mp-1073493) | 0.4445 | 0.192 | 2 |
Mg4Si3 (mp-1074466) | 0.4496 | 0.202 | 2 |
Mg4Si3 (mp-1074562) | 0.4466 | 0.187 | 2 |
MgSi (mp-1073734) | 0.4087 | 0.172 | 2 |
Mg3Si4 (mp-1075100) | 0.4516 | 0.201 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.2367 eV |
Corrected Energy-44.8883 eV
Uncorrected energy = -45.3143 eV
Composition-based energy adjustment (0.071 eV/atom x 6.0 atoms) = 0.4260 eV
Corrected energy = -44.8883 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)