Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.052 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.185 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K3Nd3I10 (mp-676864) | 0.5539 | 0.075 | 3 |
Yb7Mg3Ge8 (mp-685798) | 0.5391 | 0.256 | 3 |
Ba2LaI7 (mp-772158) | 0.5416 | 0.054 | 3 |
Na2Sr3As4 (mp-677245) | 0.5353 | 0.115 | 3 |
RbNd2I5 (mp-570360) | 0.5846 | 0.135 | 3 |
Li3VOF6 (mp-765240) | 0.7395 | 0.072 | 4 |
KSr2Cd2Sb3 (mp-866639) | 0.7419 | 0.000 | 4 |
Mg4Si3 (mp-1074404) | 0.4872 | 0.133 | 2 |
Mg4Si3 (mp-1074466) | 0.5071 | 0.202 | 2 |
MgSi (mp-1073734) | 0.4521 | 0.172 | 2 |
Mg3Si4 (mp-1075100) | 0.4481 | 0.201 | 2 |
Mg3Si4 (mp-1075203) | 0.4750 | 0.199 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.1846 eV |
Corrected Energy-44.1588 eV
Uncorrected energy = -44.5848 eV
Composition-based energy adjustment (0.071 eV/atom x 6.0 atoms) = 0.4260 eV
Corrected energy = -44.1588 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)