Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.112 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.245 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li7VP4 (mp-675045) | 0.5729 | 0.463 | 3 |
Ce3NF6 (mp-675921) | 0.5148 | 0.068 | 3 |
BaLaCl5 (mp-772035) | 0.5601 | 0.062 | 3 |
BaCaSn3 (mp-583645) | 0.5829 | 0.000 | 3 |
Pr3NF6 (mp-33319) | 0.5251 | 0.057 | 3 |
K2SrCdSb2 (mp-863758) | 0.7381 | 0.000 | 4 |
KSr2Cd2Sb3 (mp-866639) | 0.7469 | 0.000 | 4 |
Mg7Si4 (mp-1074799) | 0.4422 | 0.208 | 2 |
Mg7Si4 (mp-1074788) | 0.3591 | 0.169 | 2 |
Mg7Si4 (mp-1074923) | 0.4108 | 0.184 | 2 |
Mg5Si6 (mp-1075464) | 0.4309 | 0.236 | 2 |
Mg6Si5 (mp-1073915) | 0.4189 | 0.213 | 2 |
Rb (mp-640416) | 0.7416 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.1253 eV |
Corrected Energy-86.6568 eV
Uncorrected energy = -87.5088 eV
Composition-based energy adjustment (0.071 eV/atom x 12.0 atoms) = 0.8520 eV
Corrected energy = -86.6568 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)