material

Mg2Cu3Si

ID:

mp-10746

DOI:

10.17188/1187329


Tags: Copper magnesium silicide (3/2/1)

Material Details

Final Magnetic Moment
0.034 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.236 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.16 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 53304 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <1 1 0> <1 1 1> 0.000 143.8
ZnO (mp-2133) <0 0 1> <0 0 1> 0.000 65.5
BN (mp-984) <0 0 1> <0 0 1> 0.001 21.8
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.001 21.8
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.002 284.0
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.002 196.6
KCl (mp-23193) <1 1 1> <0 0 1> 0.003 284.0
AlN (mp-661) <0 0 1> <0 0 1> 0.003 262.1
GdScO3 (mp-5690) <0 0 1> <1 1 1> 0.006 287.6
MgO (mp-1265) <1 1 1> <0 0 1> 0.017 284.0
BN (mp-984) <1 0 1> <0 0 1> 0.017 240.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.020 196.6
SrTiO3 (mp-4651) <1 1 1> <1 0 0> 0.022 276.8
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.030 284.0
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.030 316.2
C (mp-48) <0 0 1> <0 0 1> 0.034 196.6
LiF (mp-1138) <1 0 0> <0 0 1> 0.034 349.5
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.036 118.6
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.039 262.1
LiF (mp-1138) <1 1 1> <0 0 1> 0.039 87.4
SiC (mp-8062) <1 0 0> <0 0 1> 0.040 152.9
MoSe2 (mp-1634) <1 0 1> <1 0 0> 0.042 158.2
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.043 355.9
AlN (mp-661) <1 0 0> <1 0 0> 0.044 79.1
C (mp-48) <1 1 1> <1 0 0> 0.046 237.3
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.048 196.6
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.051 237.3
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.052 316.3
InAs (mp-20305) <1 1 1> <0 0 1> 0.055 65.5
CaCO3 (mp-3953) <1 1 1> <0 0 1> 0.059 152.9
CaCO3 (mp-3953) <1 0 0> <0 0 1> 0.061 87.4
C (mp-66) <1 0 0> <0 0 1> 0.062 240.3
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.067 65.5
GaSe (mp-1943) <0 0 1> <0 0 1> 0.069 87.4
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.072 355.9
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.080 21.8
Al2O3 (mp-1143) <1 1 0> <1 1 1> 0.083 215.7
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.084 316.3
TbScO3 (mp-31119) <0 0 1> <1 1 1> 0.088 287.6
C (mp-66) <1 1 1> <0 0 1> 0.096 21.8
NdGaO3 (mp-3196) <1 1 1> <1 0 0> 0.097 276.8
CdS (mp-672) <0 0 1> <0 0 1> 0.098 196.6
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.113 197.7
Te2W (mp-22693) <0 0 1> <1 0 0> 0.118 197.7
BaF2 (mp-1029) <1 1 0> <1 0 1> 0.118 225.9
Te2W (mp-22693) <0 1 1> <1 1 1> 0.122 287.6
BN (mp-984) <1 1 1> <1 0 0> 0.128 237.3
Ni (mp-23) <1 1 0> <0 0 1> 0.133 87.4
AlN (mp-661) <1 0 1> <1 0 0> 0.139 158.2
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.139 152.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
191 57 45 0 0 0
57 191 45 0 0 0
45 45 206 0 0 0
0 0 0 54 0 0
0 0 0 0 54 0
0 0 0 0 0 67
Compliance Tensor Sij (10-12Pa-1)
5.9 -1.5 -1 0 0 0
-1.5 5.9 -1 0 0 0
-1 -1 5.3 0 0 0
0 0 0 18.6 0 0
0 0 0 0 18.6 0
0 0 0 0 0 14.9
Shear Modulus GV
64 GPa
Bulk Modulus KV
98 GPa
Shear Modulus GR
63 GPa
Bulk Modulus KR
98 GPa
Shear Modulus GVRH
64 GPa
Bulk Modulus KVRH
98 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca2Mg3Si (mp-1095343) 0.1083 0.119 3
Zr2Fe3Si (mp-16336) 0.1723 0.099 3
Nb2Co3Si (mp-10366) 0.0791 0.000 3
Na2LiAu3 (mp-12815) 0.1773 0.000 3
Mn2Co3Ge (mp-22702) 0.1535 0.140 3
CaCd2 (mp-1078) 0.0793 0.010 2
CaZn2 (mp-13364) 0.0651 0.025 2
MgAg2 (mp-1094121) 0.0833 0.110 2
CdCu2 (mp-16775) 0.0657 0.012 2
YZn2 (mp-1095495) 0.0779 0.027 2
Co (mp-1072089) 0.2792 0.199 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Cu_pv Si
Final Energy/Atom
-3.7216 eV
Corrected Energy
-44.5171 eV
Uncorrected energy = -44.6591 eV Composition-based energy adjustment (0.071 eV/atom x 2.0 atoms) = 0.1420 eV Corrected energy = -44.5171 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 53304
Submitted by
User remarks:
  • Copper magnesium silicide (3/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)