@article{PhysRevMaterials.2.023803, author = "Huan, Tran Doan", title = "Pressure-stabilized binary compounds of magnesium and silicon", journal = "Phys. Rev. Materials", volume = "2", issue = "2", pages = "023803", numpages = "7", year = "2018", month = "Feb", publisher = "American Physical Society", doi = "10.1103/PhysRevMaterials.2.023803", url = "https://link.aps.org/doi/10.1103/PhysRevMaterials.2.023803" }