material

TiFeSb

ID:

mp-10755

DOI:

10.17188/1187338


Tags: Iron titanium antimonide (1/1/1)

Material Details

Final Magnetic Moment
0.991 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FiM
Formation Energy / Atom
-0.432 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.06 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 53537 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 0 0> <1 0 0> 0.001 320.3
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.001 61.6
WS2 (mp-224) <0 0 1> <1 1 1> 0.001 61.6
InP (mp-20351) <1 1 0> <1 1 0> 0.006 50.3
InP (mp-20351) <1 1 1> <1 1 1> 0.006 61.6
InP (mp-20351) <1 0 0> <1 0 0> 0.006 35.6
Mg (mp-153) <0 0 1> <1 1 1> 0.006 61.6
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.007 320.3
LiF (mp-1138) <1 0 0> <1 0 0> 0.013 284.7
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.019 249.1
CdS (mp-672) <0 0 1> <1 1 1> 0.021 61.6
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.030 151.0
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.031 184.9
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.052 320.3
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.063 177.9
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.066 213.5
AlN (mp-661) <1 0 1> <1 1 0> 0.081 251.6
InSb (mp-20012) <1 0 0> <1 0 0> 0.085 177.9
MgO (mp-1265) <1 1 1> <1 0 0> 0.087 249.1
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.088 177.9
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.096 184.9
SiC (mp-8062) <1 1 0> <1 1 0> 0.098 301.9
CdTe (mp-406) <1 0 0> <1 0 0> 0.106 177.9
C (mp-66) <1 1 0> <1 1 0> 0.111 201.3
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.114 61.6
AlN (mp-661) <1 1 1> <1 1 0> 0.115 201.3
PbS (mp-21276) <1 1 0> <1 1 0> 0.115 50.3
PbS (mp-21276) <1 1 1> <1 1 1> 0.116 61.6
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.117 142.3
PbS (mp-21276) <1 0 0> <1 0 0> 0.119 35.6
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.123 320.3
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.134 151.0
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.136 355.8
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.136 355.8
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.140 320.3
GaN (mp-804) <0 0 1> <1 1 0> 0.141 251.6
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> 0.144 249.1
AlN (mp-661) <1 1 0> <1 1 0> 0.155 301.9
ZnO (mp-2133) <1 1 1> <1 0 0> 0.163 284.7
LaF3 (mp-905) <0 0 1> <1 1 1> 0.187 184.9
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.190 301.9
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.196 308.2
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.197 201.3
GaN (mp-804) <1 0 1> <1 0 0> 0.211 213.5
TiO2 (mp-390) <0 0 1> <1 0 0> 0.230 71.2
MgO (mp-1265) <1 1 0> <1 1 0> 0.236 50.3
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.240 284.7
MgO (mp-1265) <1 0 0> <1 0 0> 0.244 35.6
Cu (mp-30) <1 1 0> <1 1 0> 0.280 151.0
Ni (mp-23) <1 1 0> <1 1 0> 0.287 301.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
198 71 71 0 0 0
71 198 71 0 0 0
71 71 198 0 0 0
0 0 0 47 0 0
0 0 0 0 47 0
0 0 0 0 0 47
Compliance Tensor Sij (10-12Pa-1)
6.3 -1.7 -1.7 0 0 0
-1.7 6.3 -1.7 0 0 0
-1.7 -1.7 6.3 0 0 0
0 0 0 21.4 0 0
0 0 0 0 21.4 0
0 0 0 0 0 21.4
Shear Modulus GV
53 GPa
Bulk Modulus KV
114 GPa
Shear Modulus GR
52 GPa
Bulk Modulus KR
114 GPa
Shear Modulus GVRH
53 GPa
Bulk Modulus KVRH
114 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NbCoSb (mp-31460) 0.0000 0.021 3
LiMgAs (mp-12558) 0.0000 0.000 3
LiGaSi (mp-11390) 0.0000 0.071 3
YbCuGe (mp-13306) 0.0000 0.162 3
HoGeAu (mp-13308) 0.0000 0.075 3
TiF2 (mp-282) 0.0000 0.248 2
PuO2 (mp-1959) 0.0000 0.000 2
Na2Se (mp-1266) 0.0000 0.000 2
TbO2 (mp-2458) 0.0000 0.131 2
H2Se (mp-24420) 0.0000 0.645 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Fe_pv Sb
Final Energy/Atom
-7.1991 eV
Corrected Energy
-21.7893 eV
Uncorrected energy = -21.5973 eV Composition-based energy adjustment (-0.192 eV/atom x 1.0 atoms) = -0.1920 eV Corrected energy = -21.7893 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 53537
Submitted by
User remarks:
  • Iron titanium antimonide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)