Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.190 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.272 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce7(GePd2)2 (mp-683992) | 0.6308 | 0.201 | 3 |
SrLa5F17 (mp-675492) | 0.5904 | 0.023 | 3 |
Hf8MnTe6 (mp-616615) | 0.6705 | 0.005 | 3 |
Cs5(KPb6)3 (mp-581775) | 0.5465 | 0.006 | 3 |
Mn4Nb7Ge8 (mp-29906) | 0.6446 | 0.028 | 3 |
Mg2Si3 (mp-1073130) | 0.4487 | 0.295 | 2 |
Mg3Si4 (mp-1075253) | 0.4622 | 0.217 | 2 |
Mg5Si9 (mp-1075660) | 0.4332 | 0.244 | 2 |
Mg5Si9 (mp-1075734) | 0.4095 | 0.271 | 2 |
Mg5Si9 (mp-1075744) | 0.4526 | 0.268 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.8691 eV |
Corrected Energy-108.3336 eV
-108.3336 eV = -108.3336 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)