Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.116 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.198 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2In2As3 (mp-21741) | 0.6656 | 0.000 | 3 |
Li2SiN2 (mp-684024) | 0.6388 | 0.000 | 3 |
K2Cd2Te3 (mp-571637) | 0.6524 | 0.000 | 3 |
Na2GeN2 (mp-1029851) | 0.6249 | 0.000 | 3 |
Nd3S2Br5 (mp-28297) | 0.6720 | 0.020 | 3 |
Ag2Bi2S3Cl2 (mp-559071) | 0.5679 | 0.000 | 4 |
SrLiGaN2 (mp-568385) | 0.6839 | 0.000 | 4 |
K3Nb2CuSe12 (mp-6168) | 0.6910 | 0.000 | 4 |
Nb2Tl3CuSe12 (mp-570757) | 0.6423 | 0.000 | 4 |
La5S4NO2 (mp-1019896) | 0.6757 | 0.004 | 4 |
Mg5Si9 (mp-1075608) | 0.5180 | 0.210 | 2 |
Mg5Si9 (mp-1075627) | 0.5596 | 0.194 | 2 |
Mg5Si9 (mp-1075664) | 0.5251 | 0.187 | 2 |
Mg5Si9 (mp-1075592) | 0.5677 | 0.226 | 2 |
Mg5Si9 (mp-1075649) | 0.5079 | 0.188 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.9428 eV |
Corrected Energy-110.3983 eV
-110.3983 eV = -110.3983 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)