Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.019 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.156 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2Si + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrLaCl5 (mp-851090) | 0.6176 | 0.078 | 3 |
Cr2B2Ir (mp-569911) | 0.6354 | 0.060 | 3 |
Cs5(KPb6)3 (mp-581775) | 0.5937 | 0.006 | 3 |
CsNaGe2 (mp-29566) | 0.6088 | 0.000 | 3 |
Mg3Ga7Co2 (mp-571626) | 0.6102 | 0.000 | 3 |
MgSi (mp-1073721) | 0.4512 | 0.147 | 2 |
Mg4Si3 (mp-1074518) | 0.3977 | 0.176 | 2 |
Mg4Si3 (mp-1074388) | 0.4408 | 0.266 | 2 |
Mg7Si4 (mp-1074788) | 0.4025 | 0.169 | 2 |
Mg7Si4 (mp-1074923) | 0.4361 | 0.184 | 2 |
Rb (mp-640416) | 0.6277 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si |
Final Energy/Atom-3.1114 eV |
Corrected Energy-62.2280 eV
-62.2280 eV = -62.2280 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)