Final Magnetic Moment0.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.688 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.390 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK2CrO4 + KCr3O8 + Cr2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaPdO3 (mp-976968) | 0.0000 | 0.260 | 3 |
MnZnO3 (mp-1016932) | 0.0000 | 0.561 | 3 |
VCdO3 (mp-1016904) | 0.0000 | 0.285 | 3 |
MgIrO3 (mp-1016826) | 0.0000 | 0.784 | 3 |
AlCo3C (mp-10037) | 0.0000 | 0.020 | 3 |
Ba2VFeO6 (mp-1096778) | 0.0000 | 2.272 | 4 |
Ba2ScSbO6 (mp-20709) | 0.0000 | 2.196 | 4 |
Ba2YbSbO6 (mp-14223) | 0.0000 | 1.747 | 4 |
Ba2YSbO6 (mp-14226) | 0.0000 | 2.082 | 4 |
Ba2NbFeO6 (mp-1096853) | 0.0000 | 2.749 | 4 |
Ba3Sb2 (mp-1013582) | 0.0000 | 0.409 | 2 |
Mn4N (mp-505622) | 0.0000 | 0.000 | 2 |
Ba3P2 (mp-1013551) | 0.0000 | 0.446 | 2 |
Sr3Bi2 (mp-1013587) | 0.0000 | 0.373 | 2 |
Ca3As2 (mp-1096854) | 0.0000 | 0.360 | 2 |
BaLaMgBiO6 (mp-41414) | 0.0488 | 0.096 | 5 |
BaLaMgNbO6 (mp-39288) | 0.0712 | 0.090 | 5 |
SrLaNbZnO6 (mp-41918) | 0.0665 | 0.126 | 5 |
SrLaMnCoO6 (mp-40761) | 0.0404 | 0.247 | 5 |
Sr6Ca2MnFe7O24 (mp-1075969) | 0.0482 | 0.021 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.7380 | 0.065 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: K_sv Cr_pv O |
Final Energy/Atom-5.9853 eV |
Corrected Energy-33.9863 eV
Uncorrected energy = -29.9263 eV
Composition-based energy adjustment (-0.687 eV/atom x 3.0 atoms) = -2.0610 eV
Composition-based energy adjustment (-1.999 eV/atom x 1.0 atoms) = -1.9990 eV
Corrected energy = -33.9863 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)