Final Magnetic Moment2.089 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.750 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSc2Sb + Ce2Sb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GdScSi (mp-22480) | 0.1106 | 0.000 | 3 |
TbScGe (mp-4395) | 0.0824 | 0.006 | 3 |
GdScGe (mp-4796) | 0.0832 | 0.000 | 3 |
LaScSb (mp-1076970) | 0.1171 | 0.000 | 3 |
NdScSb (mp-1077443) | 0.0572 | 0.000 | 3 |
Ba2Sb (mp-9908) | 0.3215 | 0.016 | 2 |
Ba2Bi (mp-567872) | 0.3250 | 0.025 | 2 |
GdO2 (mp-21149) | 0.3148 | 0.145 | 2 |
CeS2 (mp-1018663) | 0.2404 | 0.014 | 2 |
Zr2Sb (mp-31379) | 0.3311 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Sc_sv Sb |
Final Energy/Atom-6.2144 eV |
Corrected Energy-37.6701 eV
Uncorrected energy = -37.2861 eV
Composition-based energy adjustment (-0.192 eV/atom x 2.0 atoms) = -0.3840 eV
Corrected energy = -37.6701 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)