Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.931 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.050 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaAgP (mp-9899) | 0.0049 | 0.000 | 3 |
EuZnGe (mp-1077151) | 0.0211 | 0.048 | 3 |
SrSbPt (mp-8605) | 0.0086 | 0.000 | 3 |
YbCuSi (mp-8124) | 0.0243 | 0.010 | 3 |
SrLiP (mp-10614) | 0.0175 | 0.075 | 3 |
NdGd2 (mp-582464) | 0.0219 | 1.656 | 2 |
MnB2 (mp-1000769) | 0.0263 | 0.093 | 2 |
SmGa2 (mp-477) | 0.0087 | 0.000 | 2 |
ThGa2 (mp-11419) | 0.0175 | 0.000 | 2 |
CeGa2 (mp-912227) | 0.0007 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv As Au |
Final Energy/Atom-4.2148 eV |
Corrected Energy-25.2890 eV
-25.2890 eV = -25.2890 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)