Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.160 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.050 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYTe3 + Y2Te3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
USbTe (mp-7935) | 0.2530 | 0.000 | 3 |
ThAsSe (mp-1019357) | 0.1574 | 0.000 | 3 |
ThBiTe (mp-1019362) | 0.2448 | 0.000 | 3 |
ThSbTe (mp-1019361) | 0.2013 | 0.000 | 3 |
ThPS (mp-12876) | 0.1577 | 0.000 | 3 |
TbTe2 (mp-1019324) | 0.0303 | 0.037 | 2 |
SmTe2 (mp-1019266) | 0.0359 | 0.000 | 2 |
HoTe2 (mp-1018732) | 0.0423 | 0.058 | 2 |
ErTe2 (mp-1018692) | 0.0514 | 0.068 | 2 |
DyTe2 (mp-1018679) | 0.0140 | 0.047 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Te |
Final Energy/Atom-5.4110 eV |
Corrected Energy-32.4659 eV
-32.4659 eV = -32.4659 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)