Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.075 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.057 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZr2Cu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sc3(Ga3Fe)2 (mp-30701) | 0.6001 | 0.045 | 3 |
LaInNi2 (mp-21207) | 0.5830 | 0.000 | 3 |
LuGa2Ni (mp-1025552) | 0.5980 | 0.000 | 3 |
TmGa2Ni (mp-1025504) | 0.5998 | 0.000 | 3 |
PrInNi2 (mp-1080775) | 0.5899 | 0.000 | 3 |
Na2LiGaAs2 (mp-9722) | 0.7477 | 0.000 | 4 |
MgSi (mp-1073720) | 0.5111 | 0.237 | 2 |
Mg4Si3 (mp-1074307) | 0.5339 | 0.200 | 2 |
Mg3Si4 (mp-1075111) | 0.5239 | 0.292 | 2 |
Re2P (mp-1637) | 0.5078 | 0.000 | 2 |
Mg2Bi (mp-1039091) | 0.4607 | 0.151 | 2 |
Rb (mp-656615) | 0.6627 | 0.023 | 1 |
Rb (mp-640416) | 0.7465 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv Cu_pv |
Final Energy/Atom-7.1399 eV |
Corrected Energy-42.8394 eV
Uncorrected energy = -42.8394 eV
Corrected energy = -42.8394 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)