Final Magnetic Moment0.562 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.864 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GdScSi (mp-22480) | 0.1095 | 0.000 | 3 |
TbScGe (mp-4395) | 0.0748 | 0.006 | 3 |
GdScGe (mp-4796) | 0.0784 | 0.000 | 3 |
LaScSb (mp-1076970) | 0.0804 | 0.000 | 3 |
CeScSb (mp-1077197) | 0.0572 | 0.013 | 3 |
Ba2Sb (mp-9908) | 0.3038 | 0.016 | 2 |
Ba2Bi (mp-567872) | 0.3068 | 0.025 | 2 |
GdO2 (mp-21149) | 0.3276 | 0.145 | 2 |
CeS2 (mp-1018663) | 0.2538 | 0.014 | 2 |
Zr2Sb (mp-31379) | 0.3279 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Sc_sv Sb |
Final Energy/Atom-5.9407 eV |
Corrected Energy-36.0281 eV
Uncorrected energy = -35.6441 eV
Composition-based energy adjustment (-0.192 eV/atom x 2.0 atoms) = -0.3840 eV
Corrected energy = -36.0281 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)