Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.607 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.031 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPrSi2 + Pr4Ge7 + Si |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
UCoSi (mp-20811) | 0.3971 | 0.078 | 3 |
EuZnGe (mp-1018702) | 0.3815 | 0.101 | 3 |
NdSiGe (mp-1077182) | 0.1377 | 0.042 | 3 |
LaAsIr (mp-1071028) | 0.3860 | 0.002 | 3 |
LaAsRh (mp-10956) | 0.4182 | 0.000 | 3 |
YSi2 (mp-12769) | 0.4026 | 0.020 | 2 |
PrGe2 (mp-1077183) | 0.3732 | 0.044 | 2 |
ErSi2 (mp-1077267) | 0.3991 | 0.045 | 2 |
HoSi2 (mp-1077147) | 0.3741 | 0.071 | 2 |
CeGe2 (mp-917642) | 0.3723 | 0.114 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Si Ge_d |
Final Energy/Atom-5.5497 eV |
Corrected Energy-33.2980 eV
-33.2980 eV = -33.2980 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)