Final Magnetic Moment0.035 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.396 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImm2 [44] |
HallI 2 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
EuGeAu (mp-9293) | 0.3174 | 0.000 | 3 |
YbGeAu (mp-570711) | 0.2961 | 0.000 | 3 |
YbSnAu (mp-570947) | 0.2164 | 0.000 | 3 |
CaSnAu (mp-1071278) | 0.2961 | 0.013 | 3 |
CaSnAu (mp-29561) | 0.2939 | 0.000 | 3 |
SrHg2 (mp-568526) | 0.3108 | 0.008 | 2 |
LaAg2 (mp-1025059) | 0.2595 | 0.000 | 2 |
LuZn2 (mp-1024948) | 0.3100 | 0.000 | 2 |
PrAg2 (mp-1072619) | 0.2926 | 0.000 | 2 |
EuAg2 (mp-932723) | 0.2966 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Ga_d Ag |
Final Energy/Atom-4.3272 eV |
Corrected Energy-25.9635 eV
-25.9635 eV = -25.9635 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)