Final Magnetic Moment0.016 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.764 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg2Ni3P (mp-8969) | 0.1066 | 0.000 | 3 |
Sm2GeRh3 (mp-31402) | 0.0561 | 0.000 | 3 |
Pr2SiRh3 (mp-1072391) | 0.1573 | 0.006 | 3 |
Y2GeRh3 (mp-10214) | 0.0555 | 0.000 | 3 |
Er2GeRh3 (mp-1076961) | 0.0893 | 0.000 | 3 |
NdMn2 (mp-1095569) | 0.4584 | 0.436 | 2 |
TmMn2 (mp-30786) | 0.4275 | 0.033 | 2 |
SrZn2 (mp-13365) | 0.4770 | 0.049 | 2 |
ErMn2 (mp-913259) | 0.4440 | 0.042 | 2 |
NdMn2 (mp-569334) | 0.3924 | 0.436 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Ge_d Rh_pv |
Final Energy/Atom-6.8105 eV |
Corrected Energy-40.8633 eV
-40.8633 eV = -40.8633 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)