Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.519 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.275 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiSBr + FeS |
Band Gap0.281 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaTlCl3 (mp-998787) | 0.6218 | 0.000 | 3 |
CaInBr3 (mp-28534) | 0.5890 | 0.000 | 3 |
NaMgF3 (mp-12948) | 0.6311 | 0.031 | 3 |
Ca(SnO2)2 (mvc-6573) | 0.5382 | 0.180 | 3 |
MgSiO3 (mp-4391) | 0.5954 | 0.259 | 3 |
MnSbS2Br (mp-554061) | 0.5524 | 0.014 | 4 |
MnBiS2Cl (mp-558130) | 0.5324 | 0.000 | 4 |
MnBiSe2I (mp-569109) | 0.5243 | 0.006 | 4 |
CdBiS2Br (mp-561079) | 0.5377 | 0.018 | 4 |
MnBiS2Br (mp-557805) | 0.4789 | 0.007 | 4 |
Te8Ir3 (mp-32682) | 0.7366 | 0.018 | 2 |
Mn3O4 (mp-715570) | 0.7217 | 0.053 | 2 |
Na5Ca6Nd5Zr16O48 (mp-695571) | 0.7193 | 0.004 | 5 |
Ca5La7Mn7Ru5O36 (mp-743863) | 0.6806 | 0.442 | 5 |
Ca5Yb3Ti5Mn3O24 (mp-698722) | 0.7198 | 0.008 | 5 |
Ca16Zr9Ta7N7O41 (mp-677269) | 0.7091 | 0.046 | 5 |
LaMgFeSbO6 (mvc-9012) | 0.7024 | 0.218 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Fe_pv Bi S Br |
Final Energy/Atom-4.7064 eV |
Corrected Energy-49.7183 eV
-49.7183 eV = -47.0645 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)