Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.758 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.151 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeO2 + As2O3 + As |
Band Gap0.126 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
EuSeO3 (mp-755177) | 0.3545 | 0.000 | 3 |
RbGeCl3 (mp-27369) | 0.2797 | 0.000 | 3 |
PbSeO3 (mp-20716) | 0.4528 | 0.000 | 3 |
LaAsO3 (mp-1079050) | 0.0768 | 0.000 | 3 |
SrSeO3 (mp-555098) | 0.4540 | 0.001 | 3 |
KSO2F (mp-6560) | 0.6224 | 0.000 | 4 |
RbSO2F (mp-6384) | 0.6542 | 0.000 | 4 |
LaNiSnH (mp-510577) | 0.7171 | 0.000 | 4 |
PrNiSnH (mp-510579) | 0.7166 | 0.000 | 4 |
NdNiSnH (mp-510580) | 0.7262 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce As O |
Final Energy/Atom-7.4239 eV |
Corrected Energy-78.3608 eV
Uncorrected energy = -74.2388 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Corrected energy = -78.3608 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)