Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.019 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP41212 [92] |
HallP 4abw 2nw |
Point Group422 |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiFeAs (mp-1008927) | 0.6095 | 0.296 | 3 |
EuPb (mp-20394) | 0.1153 | 0.000 | 2 |
HoHg2 (mp-1063224) | 0.2389 | 0.070 | 2 |
LaAs (mp-20494) | 0.1611 | 0.370 | 2 |
Nb3Au2 (mp-2123) | 0.2612 | 0.000 | 2 |
CaZn3 (mp-1094784) | 0.1216 | 0.121 | 2 |
Rb (mp-639755) | 0.1121 | 0.016 | 1 |
Hg (mp-569289) | 0.1389 | 0.008 | 1 |
Pr (mp-568938) | 0.1989 | 0.086 | 1 |
Sc (mp-1056366) | 0.0855 | 0.110 | 1 |
Sc (mp-1064244) | 0.2400 | 0.112 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv |
Final Energy/Atom-1.9864 eV |
Corrected Energy-15.8916 eV
-15.8916 eV = -15.8916 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)