Final Magnetic Moment0.033 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.681 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP62m [189] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZrCoSn (mp-30563) | 0.0405 | 0.000 | 3 |
SmHgPd (mp-567912) | 0.0904 | 0.000 | 3 |
TmSnIr (mp-1080427) | 0.0915 | 0.000 | 3 |
ZrGaPt (mp-1080495) | 0.0527 | 0.009 | 3 |
HoInAu (mp-3630) | 0.0696 | 0.000 | 3 |
Mg3Al9FeSi5 (mp-7062) | 0.7309 | 0.006 | 4 |
Mg3Al8FeSi6 (mp-571315) | 0.7433 | 0.141 | 4 |
SiPd2 (mp-697068) | 0.3815 | 0.000 | 2 |
USe2 (mp-8591) | 0.3616 | 0.032 | 2 |
GePd2 (mp-423) | 0.2455 | 0.000 | 2 |
K2Re (mp-1080778) | 0.3934 | 1.993 | 2 |
K2Tc (mp-1084834) | 0.3796 | 1.575 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Hg Pd |
Final Energy/Atom-4.1016 eV |
Corrected Energy-36.9143 eV
Uncorrected energy = -36.9143 eV
Corrected energy = -36.9143 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)